CHINESE JOURNAL OF ENERGETIC MATERIALS
+Advanced Search

Electric Burst Characteristic of Exploding Foil before and after Aging
Author:
Affiliation:

(1. National Key Laboratory of Applied Physics and Chemistry, Shaanxi Applied Physics and Chemistry Research Institute, Xi′an 710061, China; 2. The Rocket Force Equipment Academy, Beijing 100085, China)

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
    Abstract:

    In order to study the storage characteristic of exploding foils, the accelerated life test at high temperature of 90 ℃ and high temperature and humidity of 80 ℃, RH 95% were carried out. The appearance, morphology, burst characteristic and flyer velocity were studied by photograph, SEM, fire test and photonic doppler velocimetry(PDV) method. Results show that after aging at 80 ℃, RH 95%, the surface of exploding foil is oxidized, and the surface color changes significantly due to the Cl element and humidity, and the average resistance obviously increases from 30.3 mΩ(before aging)to 66.8 mΩ(after aging). There is no remarkable influences of high temperature(90 ℃) on burst current, burst voltage and explosion time of exploding foil. While the burst voltage and explosion time significantly decrease after aging at 80 ℃, RH 95%. The performance of exploding foil adhesion to polyimide film becomes poor after aging. The PDV test results show that with the increasing of acceleration time, the flyer velocity decreases from 3600 m·s-1 to 2100 m·s-1 at 90 ℃ and 1200 m·s-1 at 80 ℃, RH 95%. The ability to drive slapper decreases after aging. The storage condition of high temperature and humidity has a stronger effect on flyer velocity than that of high temperature.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

都振华,孙新申,张蕊,等.爆炸桥箔加速贮存前后的电爆特性[J].含能材料,2016,24(5):479-484.
DU Zhen-hua, SUN Xin-shen, ZHANG Rui, et al. Electric Burst Characteristic of Exploding Foil before and after Aging[J]. Chinese Journal of Energetic Materials,2016,24(5):479-484.

Cope
History
  • Received:July 04,2015
  • Revised:September 24,2015
  • Adopted:October 09,2015
  • Online: May 05,2016
  • Published: May 20,2016