Orthogonal Experiments of the Spray Drying Process for Spherical HMX Micro Powder Preparation
Author:
Affiliation:

(1. School of Chemical Engineering and Environment, North University of China, Taiyuan 030051, China; 2. Hubei SanJiang Space Wan Feng Technology Development Co., Ltd, Xiaogan 432100, China)

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
    Abstract:

    Using acetone as solvent, the process conditions of preparing the spherical HMX by spray drying method were optimized by the orthogonal test L9(34), and the spherical HMX obtained under the optimal condition was characterized by scanning electron microscope (SEM). The morphology of the obtained HMX was quantitatively analyzed by the scoring method. Results show that the optimal preparation conditions of the spherical HMX are inlet temperature of 70 ℃, feed rate of 1.5 mL·min-1, spraying gas flow rate of 473 L·h-1, mass fraction of 1.5%. The median particle size of the spherical HMX obtained under optimal experimental conditions is 997.56nm and the crystalline form is the β type. Compared with raw HMX, the characteristic drop height of impact sensitivity for spherical HMX is increased by 28.21 cm.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

李小东,王江,冀威,等.喷雾干燥法制备球形HMX的正交实验[J].含能材料,2016,24(5):439-443.
LI Xiao-dong, WANG Jiang, JI Wei, et al. Orthogonal Experiments of the Spray Drying Process for Spherical HMX Micro Powder Preparation[J]. Chinese Journal of Energetic Materials,2016,24(5):439-443.

Cope
History
  • Received:May 05,2015
  • Revised:September 09,2015
  • Adopted:September 09,2015
  • Online: May 05,2016
  • Published: May 20,2016