    To reduce the water content in PGDN(1, 2-propanediol dinitrate)/DBS(dibutyl sebacate) mixed solution, the effect of pressure, spraying times, material temperature and ventilation condition on dewatering effect were investigated using spraying method. The stability test was done. The results show that the water content in mixed solution can be reduced from 0.2428% to 0.0614% under the conditions of 100 g mixed solution, pressure of 0.08 MPa, material temperature of 71 ℃ and ventilation. The mass recovery of mixed solution after spaying is 100%. Abel value of mixed solution after heating for 15 min in water bath at 80 ℃ does not change, indicating that the water content in mixed solution can be reduced greatly according to the optimized parameters and this spraying method does not cause material loss or reduction of the stability of the mixed solution.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

毕晶,张小红,王中合,等.喷雾法降低PGDN和DBS混合溶液中的水含量[J].含能材料,2012,20(3):310-313.
BI Jing, ZHANG Xiao-hong, WANG Zhong-he, et al. Reducing Water Content in PGDN/DBS Solution by Spraying Method[J]. Chinese Journal of Energetic Materials,2012,20(3):310-313.

Cope
History
  • Received:August 16,2011
  • Revised:September 22,2011
  • Adopted:October 27,2011
  • Online: June 01,2012
  • Published: