    The signal of voltage, current and light required to ignite the common and superfine lead azide (LA) were studied by semiconductor bridge (SCB). Results show that the appearance time of light is shorter than the end time of the second peak, but for the common LA, it is opposite. With increasing the ignition voltage, the duration time of the second peak and appearance time of light for two kinds of samples are short. The ignition data of the two kinds of LA obtained by D-optimization show that the minimum firing voltage of superfine LA is about 50% less than that of the common LA.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

马鹏,张琳,朱顺官,等.两种粒度叠氮化铅半导体桥点火特性研究[J].含能材料,2012,20(2):198-201.
MA Peng, ZHANG Lin, ZHU Shun-guan, et al. Ignition Character of the Common and Superfine Lead Azide by Semiconductor Bridge[J]. Chinese Journal of Energetic Materials,2012,20(2):198-201.

Cope
History
  • Received:May 16,2011
  • Revised:September 16,2011
  • Adopted:October 28,2011
  • Online: April 23,2012
  • Published: