Testing and Relieving of Residual Stress for Polymer Bonded Explosive Based on TATB
Author:
Affiliation:

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
    Abstract:

    The initial residual stress of the polymer bonded explosive based on TATB and its distribution were tested by blind-hole drilling method. The effects of hole depth and time of strain record on the testing result and the effects of heating treatment on residual stress relaxation were studied. The results show that 3 mm hole depth and 10 min time of strain records are suitable experimental parameters. The residual stress reduces to about 50% and tends to be steady by heating treatment at 75 ℃ for 3 days.

    Reference
    Related
    Cited by
Article Metrics
  • PDF:
  • HTML:
  • Abstract:
  • Cited by:
Get Citation

周红萍,李敬明,李丽,等. TATB基高聚物粘结炸药残余应力的测试和消除研究[J].含能材料,2008,16(1):37-40.
ZHOU Hong-ping, LI Jing-ming, LI Li, et al. Testing and Relieving of Residual Stress for Polymer Bonded Explosive Based on TATB[J]. Chinese Journal of Energetic Materials,2008,16(1):37-40.

Cope
History
  • Received:March 28,2007
  • Revised:
  • Adopted:
  • Online: May 06,2011
  • Published: