1.中北大学机电工程学院, 山西 太原 030051;2.北京理工大学宇航学院, 北京 100081
中文作者简介:
1.School of Mechatronic Engineering, North University of China, Taiyuan 030051, China;2.School of Aerospace Engineering, Beijing Institute of Technology, Beijing 100081, China
周东谟,谢旭源,王瑞民,等. NEPE推进剂固化降温过程残余应力应变分析[J].含能材料, 2024, 32(2):193-203. DOI:10.11943/CJEM2023224.
ZHOU Dong-mo, XIE Xu-yuan, WANG Rui-min, et al. Residual Stress/Strain Analysis of NEPE Propellant under Curing and Cooling[J]. Chinese Journal of Energetic Materials, 2024, 32(2):193-203. DOI:10.11943/CJEM2023224.