CHINESE JOURNAL OF ENERGETIC MATERIALS
+高级检索
Cu箔晶体微观形貌对爆炸箔起爆器的性能影响试验研究
作者:
作者单位:

1.北京理工大学 爆炸科学与技术国家重点实验室, 北京 100081;2.陕西应用物理化学研究所 应用物理化学国家级重点实验室, 陕西 西安 710061

作者简介:

通讯作者:

基金项目:

国家“十四五”基础科研项目(90903050301),应用物理化学国防重点实验室基金项目(6142602220102)


Effect of Micro Morphology and Crystal Structure of Copper Foil on the Performance of Exploding Foil Initiator
Author:
Affiliation:

1.State Key Laboratory of Explosion Science and Technology, Beijing Institute of Technology, Beijing 100081, China;2.Science and Technology on Applied Physical Chemistry Laboratory, Shaanxi Applied Physics and Chemistry Research Institute, Xi′an 710061, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    为研究Cu箔微观形貌及内部晶体组织结构对爆炸箔起爆器(Exploding Foil Initiator,EFI)性能的影响规律,采用闭合场非平衡磁控溅射离子镀技术和Lift-Off刻蚀法,在150,450 W和800 W溅射功率条件下制备了3种不同晶体形貌的Cu箔,并开展相应爆炸箔(Exploding Foil,EF)电爆炸性能,飞片速度以及EFI发火性能的试验研究。试验结果表明:3种溅射功率对应样品的平均晶粒尺寸分别为19.6~36.7nm,41.5~62.9 nm和58.6~80.2 nm,表面平均粗糙度分别为6.7,16.9 nm和46.2 nm,附着力分别为42.436,55.569 mN和71.135 mN。溅射功率为800 W时制备的Cu箔晶粒尺寸最大且分布最均匀,晶粒沉积致密平整,晶界较少,表面粗糙度最大,附着力最强,Cu(1 1 1)晶面的衍射峰最高,相应EF的电阻值和电感值最小,电爆炸能量利用率和飞片速度最高,集成的EFI 50%发火感度比溅射功率为450 W和150 W获得的样品分别高19.1%和22.6%。

    Abstract:

    In order to explore the effect of microstructure and crystal organization of copper (Cu) foil on the performance of exploding foil initiator(EFI), three Cu foils with different crystal morphologies were prepared through the closed-field non-equilibrium magnetron sputtering ion plating technique and Lift-Off etching method under the sputtering power of 150, 450 W and 800 W. Experimental characterizations of the electrical explosion performance and flyer velocity of exploding foil (EF), and the ignition performance of EFI were conducted subsequently. Average grain size of the samples fabricated at 150, 450 W and 800 W are 19.6-36.7nm, 41.5-62.9 nm and 58.6-80.2 nm, surface average roughness are in turn 6.7, 16.9 nm and 46.2 nm, and the adhesion force are 42.436, 55.569 mN, and 71.135 mN, respectively. Of which, the Cu foil prepared at 800 W exhibits the largest and the most uniform grain size, the densest and smoothest grain, the fewest grain boundaries, the largest surface roughness and the strongest adhesion force. The corresponding EF has the smallest resistance and inductance, highest energy conversion efficiency and flyer velocity. The 50% firing sensitivity of the integrating EFI sputtered at 800 W are 19.1% and 22.6% higher than the samples sputtered at 450 W and 150 W, respectively.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

韩克华,曾鑫,赵婉君,等. Cu箔晶体微观形貌对爆炸箔起爆器的性能影响试验研究[J].含能材料, 2023, 31(6):568-576. DOI:10.11943/CJEM2023037.
HAN Ke-hua, ZENG Xin, ZHAO Wan-jun, et al. Effect of Micro Morphology and Crystal Structure of Copper Foil on the Performance of Exploding Foil Initiator[J]. Chinese Journal of Energetic Materials, 2023, 31(6):568-576. DOI:10.11943/CJEM2023037.

复制
历史
  • 收稿日期: 2023-03-02
  • 最后修改日期: 2023-05-22
  • 录用日期: 2023-04-25
  • 在线发布日期: 2023-05-18
  • 出版日期: 2023-06-25