    摘要:

    为探究改性双基推进剂的热安全特性,采用差示扫描量热法(DSC)对黑索今(RDX)含量分别为0,18%,46%和54.6%的改性双基推进剂的热分解行为进行了研究,得到了升温速率2,5,10 ℃·min-1和20 ℃·min-1下的热分解温度。通过热反应动力学分析计算了其表观活化能、指前因子、反应速率、吉布斯自由能、活化焓及活化熵,分析了RDX含量对双基组分及表观活化能的影响规律。通过慢速烤燃和5 s爆发点试验得到不同RDX含量改性双基推进剂的响应特性。结果表明,配方中RDX含量为18%时,表观活化能最大,慢速烤燃和5 s爆发点响应温度和响应剧烈程度最低;随着RDX含量的增加,DSC第一分解峰温后移,表观活化能降低,双基推进剂的慢速烤燃响应温度向高温方向移动,体系热敏感性降低,但响应等级随之提升;当RDX含量在46%及以上时,响应等级为爆炸,不能通过慢速烤燃试验考核;5 s爆发点温度随着RDX含量的增加向高温方向移动,且上升趋势较为明显,改性双基推进剂的热安定性有所提升。

    Abstract:

    In order to explore the thermal safety characteristics of modified double base propellants, the thermal decomposition behaviors of modified double base propellants with RDX content of 0, 18%, 46% and 54.6% were studied by differential scanning calorimetry (DSC) respectively, and the thermal decomposition temperatures at different heating rates (2, 5, 10 and 20 ℃·min-1)were obtained. The apparent activation energy, activation pre-exponential factor, reaction rate, Gibbs free energy, activation enthalpy and activation entropy were calculated by thermal reaction kinetics analysis, and the influence of RDX content on the double base components and apparent activation energy was also analyzed. The response characteristics of modified double base propellants with different RDX contents were obtained by slow cook-off and 5s burst point temperature tests. Results show that when RDX content is 18%, the apparent activation energy is the highest, and the response temperature and the response intensity of slow cook-off test and 5s burst point temperatures all are the lowest. The first decomposition peak temperature of samples moved backward, the apparent activation energy decreased, the slow cook-off response temperature moved to higher temperature, the thermal sensitivity of the system decreased, but the response level increased with the increase of RDX content. The response level is explosion, which could not pass the slow cook-off test when the RDX content is 46% or above. The 5s burst point temperature moves to high temperature with the increase of RDX content and presents a significant rising trend, and the thermal stability of modified double base propellants is improved.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

程万里,高鹏,吕春玲,等. RDX含量对改性双基推进剂热安全特性的影响[J].含能材料, 2023, 31(10):1026-1034. DOI:10.11943/CJEM2022194.
CHENG Wan-li, GAO Peng, LV Chun-ling, et al. Effect of RDX Content on Thermal Safety of Modified Double base Propellant[J]. Chinese Journal of Energetic Materials, 2023, 31(10):1026-1034. DOI:10.11943/CJEM2022194.

复制
历史
  • 收稿日期: 2022-07-21
  • 最后修改日期: 2022-12-05
  • 录用日期: 2022-11-16
  • 在线发布日期: 2022-11-18
  • 出版日期: 2023-10-25