    摘要:

    为了提高锆/四氧化三铅(Zr/Pb3O4)混合药剂的混合均匀性和工艺安全性,以海藻酸钠(SA)为微胶囊黏合剂,通过液相连续流混合,在水相中利用SA与Ca2+交联生成海藻酸钙(CA)凝胶,制备了CA/Zr/Pb3O4微胶囊。对CA/Zr/Pb3O4微胶囊和传统工艺制备的NC/Zr/Pb3O4颗粒进行形貌、粒度、球形度、流散性以及假密度等表征,表明CA/Zr/Pb3O4微胶囊平均粒径为517.10 μm,方差为44.21 μm,球形度为0.90,安息角为27.44°,粒径均一,球形度良好,流散性好。对CA/Zr/Pb3O4微胶囊进行火焰感度、燃速、火焰长度以及感度测试,表明CA/Zr/Pb3O4微胶囊火焰感度为65.38 mm,低于Zr/Pb3O4粉末的81.83 mm,火焰感度有所下降;CA/Zr/Pb3O4微胶囊燃速偏差为6.86,远低于Zr/Pb3O4粉末的燃速偏差12.04,燃烧一致性好;CA/Zr/Pb3O4微胶囊的火焰长度比Zr/Pb3O4火焰长17.1 mm,粒子更多;CA/Zr/Pb3O4微胶囊的静电感度大于156.25 mJ,远大于Zr/Pb3O4粉末的0.71 mJ,静电感度有所降低,两者撞击感度都大于100 J,摩擦感度都大于360 N。制备工艺在水相中进行,安全性高且方法具有普适性,适用于多种火工药剂。

    Abstract:

    The mixing uniformity and processing safety of widely used zirconium/lead tetroxide (Zr/Pb3O4) composites are indispensable. In the current paper, a Zr/Pb3O4 microcapsule bonded with the adhesive alginate was prepared by crosslinking the liquid phase with sodium alginate(SA) and Ca2+ in aqueous phase to form calcium alginate (CA) gel. The morphology, particle size, sphericity, fluidity and apparent density of CA/Zr/Pb3O4 microcapsules and the traditional-made NC/Zr/Pb3O4 controlled sample were evaluated. The average particle size, variance, sphericity and repose angle of CA/Zr/Pb3O4 microcapsules is measured to 517.10 μm, 44.21 μm, 0.90, and 27.44°, respectively. The flame sensitivity, burning rate, flame length and sensitivity of CA/Zr/Pb3O4 microcapsules were tested to 65.38 mm, which was lower than that of Zr/Pb3O4 powder (81.83 mm). Besides, the combustion rate deviation of CA/Zr/Pb3O4 microcapsules and Zr/Pb3O4 powder is 6.86 and 12.04, respectively, implying an excellent combustion consistency. Furthermore, much more flame length of 17.1 mm and burning particles than Zr/Pb3O4 were obtained in of CA/Zr/Pb3O4 microcapsules. In addition, a reduced the electrostatic sensitivity of CA/Zr/Pb3O4 microcapsules (156.25 mJ) and Zr/Pb3O4 powder (0.71 mJ) were realized. More importantly, the water-phase preparation carried out in the current paper may pave a high-safety and universal way for a variety of pyrotechnic agents.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

韩晓丽,陈雨,祁轩,等. Zr/Pb3O4微胶囊化的制备及其性能[J].含能材料, 2022, 30(4):301-308. DOI:10.11943/CJEM2021284.
HAN Xiao-li, CHEN Yu, QI Xuan, et al. Preparation of Zr/Pb3O4 Microencapsulation and Its Property[J]. Chinese Journal of Energetic Materials, 2022, 30(4):301-308. DOI:10.11943/CJEM2021284.

复制
历史
  • 收稿日期: 2021-10-26
  • 最后修改日期: 2022-03-09
  • 录用日期: 2022-02-24
  • 在线发布日期: 2022-03-07
  • 出版日期: 2022-04-25