CHINESE JOURNAL OF ENERGETIC MATERIALS
+高级检索
镁含量对离心雾化铝镁合金粉反应性能的影响
作者:
作者单位:

1.北京理工大学 爆炸科学与技术重点实验室, 北京 100081;2.唐山威豪镁粉有限公司, 河北 迁安 064406

作者简介:

通讯作者:

基金项目:

博士后基金面上资助项目(2021M690376),国家自然科学基金委员会资助项目(21905024)


Effect of Magnesium Content on Reactive Properties of Centrifugal Atomized Aluminum-magnesium Alloy Powder
Author:
Affiliation:

1.State Key Laboratory of Explosion Science and Technology, Beijing Institute of Technology, Beijing 100081, China;2.Tangshan Weihao Magnesium Powder Co.,Ltd, Qian′an 064406, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
    摘要:

    为研究镁(Mg)含量对系列离心雾化铝镁(Al-Mg)合金粉性能的影响,选用不同Al与Mg质量投料比(70∶30、50∶50、30∶70)的离心雾化Al-Mg合金粉(Al-Mg30、Al-Mg50、Al-Mg70),采用粒度分布仪、扫描电子显微镜(SEM)、X射线粉末衍射仪(XRD)和热重分析-差示扫描量热法(TG-DSC)对合金粉进行粒度、形貌、物相和动力学研究。同时在71 ℃热氧化作用下,研究不同Mg含量对合金活性的影响。结果表明,3种Al-Mg合金粉粒度分布均匀,形貌规整,具有良好的球形度。Al-Mg30,Al-Mg50合金粉都为枝晶组织,Al-Mg70是由α固溶体和枝状析出相组成;Al-Mg合金粉物相主要是α-Al,β-Al3Mg2γ-Al12Mg17,且随着Mg含量的增加,合金化合物中β-Al3Mg2相逐渐减少,γ-Al12Mg17相逐渐增多,失活率逐渐增高,且所有Al-Mg合金粉失活率在48 h以后基本保持不变。TG-DSC结果表明,随着Mg含量的增加,合金粉的初始放热温度逐渐减小,活化能也逐渐减小,反应速率逐渐加快,3种Al-Mg合金增重比例均大于相同粒径的Mg粉(53.02%)和Al粉(8.65%)。激光点火结果表明,3种Al-Mg合金粉点火延迟时间远短于单质Al,且在燃烧过程中存在微爆现象,可显著缩短燃烧时间,且随着Mg含量增加,燃烧时间逐渐变短。

    Abstract:

    To investigate the effect of Mg content on the properties of centrifugal atomized aluminum-magnesium (Al-Mg) alloy powders, Al-Mg alloy powders with different mass ratios (70∶30, 50∶50, 30∶70) were prepared by centrifugal atomization. The particle size, morphology, physical phase, and kinetics parameters of the samples were characterized via the particle size distribution meter, scanning electron microscope (SEM), X-ray powder diffractometer (XRD) and TG-DSC. The effect of different Mg content on the activity of the alloy was also studied by thermal oxidation at 71 ℃. Results showed that all Al-Mg alloy powders had a good size distribution, regular morphology and high sphericity. The metallographic structure demonstrated that Al-Mg30 and Al-Mg50 had a dendritic structure, and Al-Mg70 was composed of α-solid solution and dendritic precipitates. The main phase of the alloy was α-Al, β-Al3Mg2 and γ-Al12Mg17. The β-Al3Mg2 phase gradually decreased and the γ-Al12Mg17 phase increased with the increasement of Mg content. Moreover, the deactivation rate of Al-Mg alloy powders was found to increase with the increasement of Mg content. The activity of alloy powders remained basically constant after 48 h. The TG-DSC results indicated that both the initial exothermic temperature and the activation energy of the alloys were gradually reduced as the Mg content increased, but the reactive speed was accelerated. The increasement ratio of weight of all Al-Mg alloys was greater than that of micron Mg (53.06%) and Al (8.63%). The results of Laser ignition showed that the ignition delay of Al-Mg alloy was much shorter than monolithic aluminum, as well as the combustion duration. The microburst phenomenon was observed in the test.

    参考文献
    相似文献
    引证文献
文章指标
  • PDF下载次数:
  • HTML阅读次数:
  • 摘要点击次数:
  • 引用次数:
引用本文

李建新,赵婉君,闫石,等.镁含量对离心雾化铝镁合金粉反应性能的影响[J].含能材料, 2021, 29(10):888-896. DOI:10.11943/CJEM2021197.
LI Jian-xin, ZHAO Wan-jun, YAN Shi, et al. Effect of Magnesium Content on Reactive Properties of Centrifugal Atomized Aluminum-magnesium Alloy Powder[J]. Chinese Journal of Energetic Materials, 2021, 29(10):888-896. DOI:10.11943/CJEM2021197.

复制
历史
  • 收稿日期: 2021-07-30
  • 最后修改日期: 2021-09-08
  • 录用日期: 2021-08-22
  • 在线发布日期: 2021-09-03
  • 出版日期: 2021-10-25